Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 35 % Show Material materials with Dehnung A50 of 35 % |
Streckgrenze Rp0,5 | 20.0 °C | 195 - 250 MPa Show Material materials with Streckgrenze Rp0,5 of 195 - 250 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 180 - 235 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 180 - 235 MPa |
Zugfestigkeit | 20.0 °C | 450 - 515 MPa Show Material materials with Zugfestigkeit of 450 - 515 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 6 - 7.5 % Show Material materials with Aluminium of 6 - 7.5 % |
Blei | 0.01 % Show Material materials with Blei of 0.01 % |
Eisen | 2 - 3 % Show Material materials with Eisen of 2 - 3 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Nickel | 0.15 % Show Material materials with Nickel of 0.15 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 0.1 % Show Material materials with Zink of 0.1 % |
Zinn | 0.2 - 0.5 % Show Material materials with Zinn of 0.2 - 0.5 % |