Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 35 % Show Material materials with Dehnung A50 of 35 % |
Streckgrenze Rp0,5 | 20.0 °C | 105 MPa Show Material materials with Streckgrenze Rp0,5 of 105 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 105 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 105 MPa |
Zugfestigkeit | 20.0 °C | 310 MPa Show Material materials with Zugfestigkeit of 310 MPa |
Chemical properties
Property | Value |
---|---|
Blei | 0.07 % Show Material materials with Blei of 0.07 % |
Eisen | 0.06 % Show Material materials with Eisen of 0.06 % |
Kupfer | 70 - 73 % Show Material materials with Kupfer of 70 - 73 % |
Zinn | 0.8 - 1.2 % Show Material materials with Zinn of 0.8 - 1.2 % |