Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 35 % Show Material materials with Dehnung A50 of 35 % |
Streckgrenze Rp0,5 | 20.0 °C | 195 - 205 MPa Show Material materials with Streckgrenze Rp0,5 of 195 - 205 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 180 - 195 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 180 - 195 MPa |
Zugfestigkeit | 20.0 °C | 450 - 485 MPa Show Material materials with Zugfestigkeit of 450 - 485 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 6 - 8 % Show Material materials with Aluminium of 6 - 8 % |
Blei | 0.01 % Show Material materials with Blei of 0.01 % |
Eisen | 1.5 - 3.5 % Show Material materials with Eisen of 1.5 - 3.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Zink | 0.2 % Show Material materials with Zink of 0.2 % |