Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 10 % Show Material materials with Dehnung A50 of 10 % |
Streckgrenze Rp0,5 | 20.0 °C | 205 - 250 MPa Show Material materials with Streckgrenze Rp0,5 of 205 - 250 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 195 - 235 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 195 - 235 MPa |
Zugfestigkeit | 20.0 °C | 550 - 620 MPa Show Material materials with Zugfestigkeit of 550 - 620 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 9 - 11 % Show Material materials with Aluminium of 9 - 11 % |
Eisen | 2 - 4 % Show Material materials with Eisen of 2 - 4 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Nickel | 4 - 5.5 % Show Material materials with Nickel of 4 - 5.5 % |
Zink | 0.3 % Show Material materials with Zink of 0.3 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |