Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 30 % Show Material materials with Dehnung A50 of 30 % |
Streckgrenze Rp0,5 | 20.0 °C | 125 - 140 MPa Show Material materials with Streckgrenze Rp0,5 of 125 - 140 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 125 - 140 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 125 - 140 MPa |
Zugfestigkeit | 20.0 °C | 310 - 345 MPa Show Material materials with Zugfestigkeit of 310 - 345 MPa |
Chemical properties
Property | Value |
---|---|
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.4 - 1 % Show Material materials with Eisen of 0.4 - 1 % |
Kupfer | 65 % Show Material materials with Kupfer of 65 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 29 - 33 % Show Material materials with Nickel of 29 - 33 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |