Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 2 - 8 % Show Material materials with Dehnung A50 of 2 - 8 % | |
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Hardness, Rockwell Superficial 15-T | 23.0 °C | 90 - 94 [-] Show Material materials with Hardness, Rockwell Superficial 15-T of 90 - 94 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 77 - 83 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 77 - 83 [-] | |
Härte, Rockwell B | 23.0 °C | 88 - 104 [-] Show Material materials with Härte, Rockwell B of 88 - 104 [-] | |
Zugfestigkeit | 23.0 °C | 585 - 895 MPa Show Material materials with Zugfestigkeit of 585 - 895 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Schmelzpunkt | 855 - 1090 °C Show Material materials with Schmelzpunkt of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.2 % Show Material materials with Aluminium of 0.2 % |
Beryllium | 1.6 - 1.85 % Show Material materials with Beryllium of 1.6 - 1.85 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |