Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 16 % Show Material materials with Dehnung A50 of 16 % | |
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Hardness, Rockwell Superficial 15-N | 23.0 °C | 67.5 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 67.5 [-] | |
Hardness, Rockwell Superficial 30-N | 23.0 °C | 37 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 37 [-] | |
Härte, Rockwell B | 23.0 °C | 95 [-] Show Material materials with Härte, Rockwell B of 95 [-] | |
Streckgrenze | 23.0 °C | 485 - 660 MPa Show Material materials with Streckgrenze of 485 - 660 MPa | |
Zugfestigkeit | 23.0 °C | 690 - 760 MPa Show Material materials with Zugfestigkeit of 690 - 760 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Schmelzpunkt | 855 - 1090 °C Show Material materials with Schmelzpunkt of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |