Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.47 g/cm³ Show Material materials with Dichte of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % | |
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass |
Streckgrenze Rp0,5 | 23.0 °C | 172 MPa Show Material materials with Streckgrenze Rp0,5 of 172 MPa | |
Zugfestigkeit | 23.0 °C | 448 MPa Show Material materials with Zugfestigkeit of 448 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 - 1.9E-5 1/K | Typical for Cast Copper Brass Yellow Brass |
Schmelzpunkt | 905 - 932 °C Show Material materials with Schmelzpunkt of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass | |
Spezifische Wärmekapazität | 23.0 °C | 335 - 390 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Wärmeleitfähigkeit | 23.0 °C | 116 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 - 1.5 % Show Material materials with Aluminium of 0.5 - 1.5 % |
Blei | 0.4 % Show Material materials with Blei of 0.4 % |
Eisen | 0.4 - 2 % Show Material materials with Eisen of 0.4 - 2 % |
Kupfer | 55 - 60 % Show Material materials with Kupfer of 55 - 60 % |
Mangan | 0.1 - 1.5 % Show Material materials with Mangan of 0.1 - 1.5 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Zink | 36 - 42 % Show Material materials with Zink of 36 - 42 % |
Zinn | 1 % Show Material materials with Zinn of 1 % |