Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 5 % Show Material materials with Dehnung A50 of 5 % |
Härte, Brinell | 20.0 °C | 200 [-] Show Material materials with Härte, Brinell of 200 [-] |
Streckgrenze Rp0,5 | 20.0 °C | 415 MPa Show Material materials with Streckgrenze Rp0,5 of 415 MPa |
Zugfestigkeit | 20.0 °C | 760 MPa Show Material materials with Zugfestigkeit of 760 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 10 - 11.5 % Show Material materials with Aluminium of 10 - 11.5 % |
Eisen | 3 - 5 % Show Material materials with Eisen of 3 - 5 % |
Kupfer | 78 % Show Material materials with Kupfer of 78 % |
Mangan | 3.5 % Show Material materials with Mangan of 3.5 % |
Nickel | 3 - 5.5 % Show Material materials with Nickel of 3 - 5.5 % |