Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 35 % Show Material materials with Dehnung A50 of 35 % |
Hardness, Rockwell F | 20.0 °C | 40 [-] Show Material materials with Hardness, Rockwell F of 40 [-] |
Streckgrenze Rp0,5 | 20.0 °C | 85 MPa Show Material materials with Streckgrenze Rp0,5 of 85 MPa |
Zugfestigkeit | 20.0 °C | 235 MPa Show Material materials with Zugfestigkeit of 235 MPa |
Chemical properties
Property | Value |
---|---|
Kupfer | 99.9 % Show Material materials with Kupfer of 99.9 % |
Phosphor | 0 - 0.01 % Show Material materials with Phosphor of 0 - 0.01 % |
Tellur | 0.4 - 0.7 % Show Material materials with Tellur of 0.4 - 0.7 % |