Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 40 % Show Material materials with Dehnung A50 of 40 % |
Härte, Rockwell B | 20.0 °C | 45 [-] Show Material materials with Härte, Rockwell B of 45 [-] |
Streckgrenze Rp0,5 | 20.0 °C | 160 MPa Show Material materials with Streckgrenze Rp0,5 of 160 MPa |
Zugfestigkeit | 20.0 °C | 400 MPa Show Material materials with Zugfestigkeit of 400 MPa |
Chemical properties
Property | Value |
---|---|
Blei | 0.25 - 0.7 % Show Material materials with Blei of 0.25 - 0.7 % |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % |
Kupfer | 58 - 61 % Show Material materials with Kupfer of 58 - 61 % |
Zinn | 0.25 % Show Material materials with Zinn of 0.25 % |