Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 32 % Show Material materials with Dehnung A50 of 32 % |
Härte, Rockwell B | 20.0 °C | 82 [-] Show Material materials with Härte, Rockwell B of 82 [-] |
Streckgrenze Rp0,5 | 20.0 °C | 255 MPa Show Material materials with Streckgrenze Rp0,5 of 255 MPa |
Zugfestigkeit | 20.0 °C | 565 MPa Show Material materials with Zugfestigkeit of 565 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 8.5 - 10 % Show Material materials with Aluminium of 8.5 - 10 % |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 3 - 4.5 % Show Material materials with Eisen of 3 - 4.5 % |
Zink | 0.8 % Show Material materials with Zink of 0.8 % |
Zinn | 0.6 % Show Material materials with Zinn of 0.6 % |