Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 35 % Show Material materials with Dehnung A50 of 35 % |
Härte, Rockwell B | 20.0 °C | 77 [-] Show Material materials with Härte, Rockwell B of 77 [-] |
Streckgrenze Rp0,5 | 20.0 °C | 285 MPa Show Material materials with Streckgrenze Rp0,5 of 285 MPa |
Zugfestigkeit | 20.0 °C | 570 MPa Show Material materials with Zugfestigkeit of 570 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 6.3 - 7 % Show Material materials with Aluminium of 6.3 - 7 % |
Arsen | 0.09 % Show Material materials with Arsen of 0.09 % |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % |
Silizium | 1.5 - 2 % Show Material materials with Silizium of 1.5 - 2 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |