Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 33 % Show Material materials with Dehnung A50 of 33 % |
Härte, Rockwell B | 20.0 °C | 69 [-] Show Material materials with Härte, Rockwell B of 69 [-] |
Streckgrenze Rp0,5 | 20.0 °C | 235 MPa Show Material materials with Streckgrenze Rp0,5 of 235 MPa |
Zugfestigkeit | 20.0 °C | 495 MPa Show Material materials with Zugfestigkeit of 495 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.25 % Show Material materials with Aluminium of 0.25 % |
Blei | 0.2 % Show Material materials with Blei of 0.2 % |
Eisen | 0.8 - 2 % Show Material materials with Eisen of 0.8 - 2 % |
Kupfer | 57 - 60 % Show Material materials with Kupfer of 57 - 60 % |
Mangan | 0.05 - 0.5 % Show Material materials with Mangan of 0.05 - 0.5 % |
Zinn | 0.5 - 1.5 % Show Material materials with Zinn of 0.5 - 1.5 % |