Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 25 % Show Material materials with Dehnung A50 of 25 % |
Härte, Rockwell B | 20.0 °C | 73 [-] Show Material materials with Härte, Rockwell B of 73 [-] |
Streckgrenze Rp0,5 | 20.0 °C | 250 MPa Show Material materials with Streckgrenze Rp0,5 of 250 MPa |
Zugfestigkeit | 20.0 °C | 570 MPa Show Material materials with Zugfestigkeit of 570 MPa |