Mechanisch
Chemical properties
Property | Value |
---|---|
Blei | 0.01 % Show Material materials with Blei of 0.01 % |
Eisen | 0.25 - 1.5 % Show Material materials with Eisen of 0.25 - 1.5 % |
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Nickel | 28 - 32 % Show Material materials with Nickel of 28 - 32 % |
Niobium | 0.5 - 1.5 % Show Material materials with Niobium of 0.5 - 1.5 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |