Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.95 g/cm³ Show Material materials with Dichte of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 120 - 156 GPa Show Material materials with Elastizitätsmodul of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 45 - 70 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 45 - 70 [-] | |
Streckgrenze Rp0,5 | 23.0 °C | 240 MPa Show Material materials with Streckgrenze Rp0,5 of 240 MPa | |
Zugfestigkeit | 23.0 °C | 310 MPa Show Material materials with Zugfestigkeit of 310 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Schmelzpunkt | 915 - 1240 °C Show Material materials with Schmelzpunkt of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade | |
Spezifische Wärmekapazität | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Wärmeleitfähigkeit | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Chemical properties