Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.95 g/cm³ Show Material materials with Dichte of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 120 - 156 GPa Show Material materials with Elastizitätsmodul of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 55 - 70 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 55 - 70 [-] | |
Streckgrenze Rp0,5 | 23.0 °C | 290 MPa Show Material materials with Streckgrenze Rp0,5 of 290 MPa | |
Zugfestigkeit | 23.0 °C | 330 MPa Show Material materials with Zugfestigkeit of 330 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Schmelzpunkt | 915 - 1240 °C Show Material materials with Schmelzpunkt of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade | |
Spezifische Wärmekapazität | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Wärmeleitfähigkeit | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Chrom | 0.3 - 0.7 % Show Material materials with Chrom of 0.3 - 0.7 % |
Eisen | 0.5 - 1 % Show Material materials with Eisen of 0.5 - 1 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 15 - 18 % Show Material materials with Nickel of 15 - 18 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Zink | 1 % Show Material materials with Zink of 1 % |