Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 8.62 g/cm³ Show Material materials with Dichte of 8.62 g/cm³ | Predicted Value |
Korngröße | 0.031 μm Show Material materials with Korngröße of 0.031 μm | Predicted Value |
Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Dauerfestigkeit | 395 MPa Show Material materials with Dauerfestigkeit of 395 MPa | Predicted Value | ||
Druckfestigkeit | 1215 MPa Show Material materials with Druckfestigkeit of 1215 MPa | Predicted Value | ||
Elastizitätsmodul | 96 - 120 GPa Show Material materials with Elastizitätsmodul of 96 - 120 GPa | Typical for Cast Copper Bronze | ||
Flächenreduzierung | 58.4 % Show Material materials with Flächenreduzierung of 58.4 % | Predicted Value | ||
Hardness, Rockwell F | 80 [-] Show Material materials with Hardness, Rockwell F of 80 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 15-N | 73 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 73 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-N | 45 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 45 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-T | 55 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 55 [-] | Predicted Value | ||
Härte, Brinell | 110 [-] Show Material materials with Härte, Brinell of 110 [-] | Predicted Value | ||
Härte, HBW | 249.8 [-] Show Material materials with Härte, HBW of 249.8 [-] | Predicted Value | ||
Härte, Vickers | 129 [-] Show Material materials with Härte, Vickers of 129 [-] | Predicted Value | ||
Poissonzahl | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Bronze | ||
Scherfestigkeit | 236.7 MPa Show Material materials with Scherfestigkeit of 236.7 MPa | Predicted Value | ||
Schubmodule | 45.0 GPa Show Material materials with Schubmodule of 45.0 GPa | Predicted Value | ||
Zugfestigkeit | 276 MPa Show Material materials with Zugfestigkeit of 276 MPa | ASTM B505 | Casting |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 1.9e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Schmelzpunkt | 760 - 1060 °C Show Material materials with Schmelzpunkt of 760 - 1060 °C | Typical for Cast Copper Bronze |
Spezifische Wärmekapazität | 376 - 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Wärmeleitfähigkeit | 12 - 81 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Elektrisch
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 0.005 % Show Material materials with Aluminium of 0.005 % | ASTM B505 | Casting |
Antimon | 0.2 % Show Material materials with Antimon of 0.2 % | ASTM B505 | Casting |
Blei | 0.5 % Show Material materials with Blei of 0.5 % | ASTM B505 | Casting |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % | ASTM B505 | Casting |
Kupfer | 88 - 90 % Show Material materials with Kupfer of 88 - 90 % | ASTM B505 | Casting |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % | ASTM B505 | Casting |
Phosphor | 1.5 % Show Material materials with Phosphor of 1.5 % | ASTM B505 | Casting |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % | ASTM B505 | Casting |
Silizium | 0.005 % Show Material materials with Silizium of 0.005 % | ASTM B505 | Casting |
Zink | 0.5 % Show Material materials with Zink of 0.5 % | ASTM B505 | Casting |
Zinn | 10 - 12 % Show Material materials with Zinn of 10 - 12 % | ASTM B505 | Casting |