Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 8.622 g/cm³ Show Material materials with Dichte of 8.622 g/cm³ | Predicted Value |
Korngröße | 0.0309 μm Show Material materials with Korngröße of 0.0309 μm | Predicted Value |
Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Dauerfestigkeit | 392 MPa Show Material materials with Dauerfestigkeit of 392 MPa | Predicted Value | ||
Druckfestigkeit | 1215 MPa Show Material materials with Druckfestigkeit of 1215 MPa | Predicted Value | ||
Elastizitätsmodul | 96 - 120 GPa Show Material materials with Elastizitätsmodul of 96 - 120 GPa | Typical for Cast Copper Bronze | ||
Flächenreduzierung | 57.3 % Show Material materials with Flächenreduzierung of 57.3 % | Predicted Value | ||
Hardness, Rockwell F | 77 [-] Show Material materials with Hardness, Rockwell F of 77 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 15-N | 73 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 73 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-N | 45 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 45 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-T | 52 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 52 [-] | Predicted Value | ||
Härte, Brinell | 107 [-] Show Material materials with Härte, Brinell of 107 [-] | Predicted Value | ||
Härte, HBW | 249.7 [-] Show Material materials with Härte, HBW of 249.7 [-] | Predicted Value | ||
Härte, Vickers | 127 [-] Show Material materials with Härte, Vickers of 127 [-] | Predicted Value | ||
Poissonzahl | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Bronze | ||
Scherfestigkeit | 224.1 MPa Show Material materials with Scherfestigkeit of 224.1 MPa | Predicted Value | ||
Schubmodule | 46.0 GPa Show Material materials with Schubmodule of 46.0 GPa | Predicted Value | ||
Zugfestigkeit | 252 MPa Show Material materials with Zugfestigkeit of 252 MPa | ASTM B505 | Casting |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 1.9e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Schmelzpunkt | 760 - 1060 °C Show Material materials with Schmelzpunkt of 760 - 1060 °C | Typical for Cast Copper Bronze |
Spezifische Wärmekapazität | 376 - 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Wärmeleitfähigkeit | 12 - 81 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Elektrisch
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 0.005 % Show Material materials with Aluminium of 0.005 % | ASTM B505 | Casting |
Antimon | 0.25 % Show Material materials with Antimon of 0.25 % | ASTM B505 | Casting |
Blei | 1 - 2.5 % Show Material materials with Blei of 1 - 2.5 % | ASTM B505 | Casting |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % | ASTM B505 | Casting |
Kupfer | 86 - 89 % Show Material materials with Kupfer of 86 - 89 % | ASTM B505 | Casting |
Nickel | 1 % Show Material materials with Nickel of 1 % | ASTM B505 | Casting |
Phosphor | 1.5 % Show Material materials with Phosphor of 1.5 % | ASTM B505 | Casting |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % | ASTM B505 | Casting |
Silizium | 0.005 % Show Material materials with Silizium of 0.005 % | ASTM B505 | Casting |
Zink | 0.7 % Show Material materials with Zink of 0.7 % | ASTM B505 | Casting |
Zinn | 9 - 11 % Show Material materials with Zinn of 9 - 11 % | ASTM B505 | Casting |