Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.677 g/cm³ Show Material materials with Dichte of 7.677 g/cm³ | Predicted Value |
Korngröße | 0.0293 μm Show Material materials with Korngröße of 0.0293 μm | Predicted Value |
Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Dauerfestigkeit | 404 MPa Show Material materials with Dauerfestigkeit of 404 MPa | Predicted Value | ||
Druckfestigkeit | 1201 MPa Show Material materials with Druckfestigkeit of 1201 MPa | Predicted Value | ||
Elastizitätsmodul | 96 - 120 GPa Show Material materials with Elastizitätsmodul of 96 - 120 GPa | Typical for Cast Copper Bronze | ||
Flächenreduzierung | 47.0 % Show Material materials with Flächenreduzierung of 47.0 % | Predicted Value | ||
Hardness, Rockwell F | 75 [-] Show Material materials with Hardness, Rockwell F of 75 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 15-N | 70 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 70 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-N | 43 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 43 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-T | 67 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 67 [-] | Predicted Value | ||
Härte, Brinell | 141 [-] Show Material materials with Härte, Brinell of 141 [-] | Predicted Value | ||
Härte, HBW | 259.7 [-] Show Material materials with Härte, HBW of 259.7 [-] | Predicted Value | ||
Härte, Vickers | 143 [-] Show Material materials with Härte, Vickers of 143 [-] | Predicted Value | ||
Poissonzahl | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Bronze | ||
Scherfestigkeit | 317.8 MPa Show Material materials with Scherfestigkeit of 317.8 MPa | Predicted Value | ||
Schubmodule | 43.5 GPa Show Material materials with Schubmodule of 43.5 GPa | Predicted Value | ||
Zugfestigkeit | 469 MPa Show Material materials with Zugfestigkeit of 469 MPa | ASTM B505 | Casting |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 1.9e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Schmelzpunkt | 760 - 1060 °C Show Material materials with Schmelzpunkt of 760 - 1060 °C | Typical for Cast Copper Bronze |
Spezifische Wärmekapazität | 376 - 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Wärmeleitfähigkeit | 12 - 81 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Elektrisch
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 8.5 - 9.5 % Show Material materials with Aluminium of 8.5 - 9.5 % | ASTM B505 | Casting |
Eisen | 2.5 - 4 % Show Material materials with Eisen of 2.5 - 4 % | ASTM B505 | Casting |
Kupfer | 86 % Show Material materials with Kupfer of 86 % | ASTM B505 | Casting |