Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.692 g/cm³ Show Material materials with Dichte of 7.692 g/cm³ | Predicted Value |
Korngröße | 0.031 μm Show Material materials with Korngröße of 0.031 μm | Predicted Value |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dauerfestigkeit | 384 MPa Show Material materials with Dauerfestigkeit of 384 MPa | Predicted Value | |||
Druckfestigkeit | 1181 MPa Show Material materials with Druckfestigkeit of 1181 MPa | Predicted Value | |||
Elastizitätsmodul | 96 - 120 GPa Show Material materials with Elastizitätsmodul of 96 - 120 GPa | Typical for Cast Copper Bronze | |||
Flächenreduzierung | 43.7 % Show Material materials with Flächenreduzierung of 43.7 % | Predicted Value | |||
Hardness, Rockwell F | 77 [-] Show Material materials with Hardness, Rockwell F of 77 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 15-N | 71 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 71 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 30-N | 44 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 44 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 30-T | 68 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 68 [-] | Predicted Value | |||
Härte, Brinell | 152 [-] Show Material materials with Härte, Brinell of 152 [-] | Predicted Value | |||
Härte, HBW | 235 [-] Show Material materials with Härte, HBW of 235 [-] | Predicted Value | |||
Härte, Vickers | 168 [-] Show Material materials with Härte, Vickers of 168 [-] | Predicted Value | |||
Poissonzahl | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Bronze | |||
Scherfestigkeit | 296.2 MPa Show Material materials with Scherfestigkeit of 296.2 MPa | Predicted Value | |||
Schubmodule | 45.0 GPa Show Material materials with Schubmodule of 45.0 GPa | Predicted Value | |||
Zugfestigkeit | 552 MPa Show Material materials with Zugfestigkeit of 552 MPa | HT, Heat-Treated | ASTM B505 | Casting |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 1.9e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Schmelzpunkt | 760 - 1060 °C Show Material materials with Schmelzpunkt of 760 - 1060 °C | Typical for Cast Copper Bronze |
Spezifische Wärmekapazität | 376 - 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Wärmeleitfähigkeit | 12 - 81 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 9 - 11 % Show Material materials with Aluminium of 9 - 11 % | HT, Heat-Treated | ASTM B505 | Casting |
Eisen | 0.8 - 1.5 % Show Material materials with Eisen of 0.8 - 1.5 % | HT, Heat-Treated | ASTM B505 | Casting |
Kupfer | 86 % Show Material materials with Kupfer of 86 % | HT, Heat-Treated | ASTM B505 | Casting |