Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.681 g/cm³ Show Material materials with Dichte of 7.681 g/cm³ | Predicted Value |
Korngröße | 0.0314 μm Show Material materials with Korngröße of 0.0314 μm | Predicted Value |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dauerfestigkeit | 382 MPa Show Material materials with Dauerfestigkeit of 382 MPa | Predicted Value | |||
Druckfestigkeit | 1183 MPa Show Material materials with Druckfestigkeit of 1183 MPa | Predicted Value | |||
Elastizitätsmodul | 96 - 120 GPa Show Material materials with Elastizitätsmodul of 96 - 120 GPa | Typical for Cast Copper Bronze | |||
Flächenreduzierung | 34.0 % Show Material materials with Flächenreduzierung of 34.0 % | Predicted Value | |||
Hardness, Rockwell F | 79 [-] Show Material materials with Hardness, Rockwell F of 79 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 15-N | 73 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 73 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 30-N | 46 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 46 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 30-T | 81 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 81 [-] | Predicted Value | |||
Härte, Brinell | 184 [-] Show Material materials with Härte, Brinell of 184 [-] | Predicted Value | |||
Härte, HBW | 241.5 [-] Show Material materials with Härte, HBW of 241.5 [-] | Predicted Value | |||
Härte, Vickers | 199 [-] Show Material materials with Härte, Vickers of 199 [-] | Predicted Value | |||
Poissonzahl | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Bronze | |||
Scherfestigkeit | 346.2 MPa Show Material materials with Scherfestigkeit of 346.2 MPa | Predicted Value | |||
Schubmodule | 45.5 GPa Show Material materials with Schubmodule of 45.5 GPa | Predicted Value | |||
Zugfestigkeit | 758 MPa Show Material materials with Zugfestigkeit of 758 MPa | HT, Heat-Treated | ASTM B505 | Casting |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 1.9e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Schmelzpunkt | 760 - 1060 °C Show Material materials with Schmelzpunkt of 760 - 1060 °C | Typical for Cast Copper Bronze |
Spezifische Wärmekapazität | 376 - 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Wärmeleitfähigkeit | 12 - 81 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 10 - 11.5 % Show Material materials with Aluminium of 10 - 11.5 % | HT, Heat-Treated | ASTM B505 | Casting |
Eisen | 3 - 5 % Show Material materials with Eisen of 3 - 5 % | HT, Heat-Treated | ASTM B505 | Casting |
Kupfer | 78 % Show Material materials with Kupfer of 78 % | HT, Heat-Treated | ASTM B505 | Casting |
Mangan | 3.5 % Show Material materials with Mangan of 3.5 % | HT, Heat-Treated | ASTM B505 | Casting |
Nickel | 3 - 5.5 % Show Material materials with Nickel of 3 - 5.5 % | HT, Heat-Treated | ASTM B505 | Casting |