Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.592 g/cm³ Show Material materials with Dichte of 7.592 g/cm³ | Predicted Value |
Korngröße | 0.0311 μm Show Material materials with Korngröße of 0.0311 μm | Predicted Value |
Mechanisch
Property | Value | Comment |
---|---|---|
Dauerfestigkeit | 376 MPa Show Material materials with Dauerfestigkeit of 376 MPa | Predicted Value |
Druckfestigkeit | 1182 MPa Show Material materials with Druckfestigkeit of 1182 MPa | Predicted Value |
Elastizitätsmodul | 96 - 120 GPa Show Material materials with Elastizitätsmodul of 96 - 120 GPa | Typical for Cast Copper Bronze |
Flächenreduzierung | 35.7 % Show Material materials with Flächenreduzierung of 35.7 % | Predicted Value |
Hardness, Rockwell F | 82 [-] Show Material materials with Hardness, Rockwell F of 82 [-] | Predicted Value |
Hardness, Rockwell Superficial 15-N | 74 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 74 [-] | Predicted Value |
Hardness, Rockwell Superficial 30-N | 47 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 47 [-] | Predicted Value |
Hardness, Rockwell Superficial 30-T | 89 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 89 [-] | Predicted Value |
Härte, Brinell | 155 [-] Show Material materials with Härte, Brinell of 155 [-] | Predicted Value |
Härte, HBW | 251.3 [-] Show Material materials with Härte, HBW of 251.3 [-] | Predicted Value |
Härte, Vickers | 236 [-] Show Material materials with Härte, Vickers of 236 [-] | Predicted Value |
Poissonzahl | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Bronze |
Scherfestigkeit | 420.7 MPa Show Material materials with Scherfestigkeit of 420.7 MPa | Predicted Value |
Schubmodule | 46.4 GPa Show Material materials with Schubmodule of 46.4 GPa | Predicted Value |
Streckgrenze | 563.7 MPa Show Material materials with Streckgrenze of 563.7 MPa | Predicted Value, RP02 |
621.1 MPa Show Material materials with Streckgrenze of 621.1 MPa | Predicted Value | |
708.3 MPa Show Material materials with Streckgrenze of 708.3 MPa | Predicted Value, RP005 |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 1.9e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Schmelzpunkt | 760 - 1060 °C Show Material materials with Schmelzpunkt of 760 - 1060 °C | Typical for Cast Copper Bronze |
Spezifische Wärmekapazität | 376 - 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Wärmeleitfähigkeit | 12 - 81 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Elektrisch
Chemical properties
Property | Value | Related Standards |
---|---|---|
Aluminium | 10.5 - 11.5 % Show Material materials with Aluminium of 10.5 - 11.5 % | ASTM B505 |
Blei | 0.03 % Show Material materials with Blei of 0.03 % | ASTM B505 |
Eisen | 4 - 5.5 % Show Material materials with Eisen of 4 - 5.5 % | ASTM B505 |
Kupfer | 74.5 % Show Material materials with Kupfer of 74.5 % | ASTM B505 |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % | ASTM B505 |
Nickel | 4.2 - 6 % Show Material materials with Nickel of 4.2 - 6 % | ASTM B505 |
Silizium | 0.15 % Show Material materials with Silizium of 0.15 % | ASTM B505 |
Zink | 0.3 % Show Material materials with Zink of 0.3 % | ASTM B505 |
Zinn | 0.25 % Show Material materials with Zinn of 0.25 % | ASTM B505 |