Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 8.47 g/cm³ Show Material materials with Dichte of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Korngröße | 0.0303 μm Show Material materials with Korngröße of 0.0303 μm | Predicted Value |
Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Dauerfestigkeit | 377 MPa Show Material materials with Dauerfestigkeit of 377 MPa | Predicted Value | ||
Druckfestigkeit | 1162 MPa Show Material materials with Druckfestigkeit of 1162 MPa | Predicted Value | ||
Elastizitätsmodul | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass | ||
Flächenreduzierung | 45.2 % Show Material materials with Flächenreduzierung of 45.2 % | Predicted Value | ||
Hardness, Rockwell F | 75 [-] Show Material materials with Hardness, Rockwell F of 75 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 15-N | 71 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 71 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-N | 43 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 43 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-T | 67 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 67 [-] | Predicted Value | ||
Härte, Brinell | 127 [-] Show Material materials with Härte, Brinell of 127 [-] | Predicted Value | ||
Härte, HBW | 244.4 [-] Show Material materials with Härte, HBW of 244.4 [-] | Predicted Value | ||
Härte, Vickers | 134 [-] Show Material materials with Härte, Vickers of 134 [-] | Predicted Value | ||
Poissonzahl | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass | ||
Scherfestigkeit | 280.1 MPa Show Material materials with Scherfestigkeit of 280.1 MPa | Predicted Value | ||
Schubmodule | 43.4 GPa Show Material materials with Schubmodule of 43.4 GPa | Predicted Value | ||
Zugfestigkeit | 414 MPa Show Material materials with Zugfestigkeit of 414 MPa | ASTM B584 | Casting |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.5e-05 - 1.9e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5e-05 - 1.9e-05 1/K | Typical for Cast Copper Brass Yellow Brass |
Schmelzpunkt | 905 - 932 °C Show Material materials with Schmelzpunkt of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass |
Spezifische Wärmekapazität | 335 - 390 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Wärmeleitfähigkeit | 116 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Elektrisch
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 0.5 - 1.5 % Show Material materials with Aluminium of 0.5 - 1.5 % | ASTM B584 | Casting |
Blei | 0.5 - 1.5 % Show Material materials with Blei of 0.5 - 1.5 % | ASTM B584 | Casting |
Eisen | 0.4 - 2 % Show Material materials with Eisen of 0.4 - 2 % | ASTM B584 | Casting |
Kupfer | 56 - 62 % Show Material materials with Kupfer of 56 - 62 % | ASTM B584 | Casting |
Mangan | 0.1 - 1 % Show Material materials with Mangan of 0.1 - 1 % | ASTM B584 | Casting |
Nickel | 1 % Show Material materials with Nickel of 1 % | ASTM B584 | Casting |
Zink | 34 - 42 % Show Material materials with Zink of 34 - 42 % | ASTM B584 | Casting |
Zinn | 0.5 - 1.5 % Show Material materials with Zinn of 0.5 - 1.5 % | ASTM B584 | Casting |