Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % | |
Elastizitätsmodul | 23.0 °C | 96 - 120 GPa Show Material materials with Elastizitätsmodul of 96 - 120 GPa | Typical for Cast Copper Bronze |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Bronze |
Streckgrenze Rp0,5 | 23.0 °C | 103 MPa Show Material materials with Streckgrenze Rp0,5 of 103 MPa | |
Zugfestigkeit | 23.0 °C | 225 MPa Show Material materials with Zugfestigkeit of 225 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.9E-5 1/K | Typical for Cast Copper Bronze |
Schmelzpunkt | 760 - 1060 °C Show Material materials with Schmelzpunkt of 760 - 1060 °C | Typical for Cast Copper Bronze | |
Spezifische Wärmekapazität | 23.0 °C | 376 - 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Wärmeleitfähigkeit | 23.0 °C | 12 - 81 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Chemical properties
Property | Value |
---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % |
Antimon | 0.2 % Show Material materials with Antimon of 0.2 % |
Blei | 1.7 - 2.5 % Show Material materials with Blei of 1.7 - 2.5 % |
Eisen | 0.25 % Show Material materials with Eisen of 0.25 % |
Kupfer | 86 - 89 % Show Material materials with Kupfer of 86 - 89 % |
Nickel | 0.7 - 1 % Show Material materials with Nickel of 0.7 - 1 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % |
Silizium | 5E-3 % Show Material materials with Silizium of 5E-3 % |
Zink | 3 - 4.5 % Show Material materials with Zink of 3 - 4.5 % |
Zinn | 4.5 - 5.5 % Show Material materials with Zinn of 4.5 - 5.5 % |