Mechanisch
Chemical properties
Property | Value |
---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % |
Antimon | 0.15 % Show Material materials with Antimon of 0.15 % |
Blei | 0.09 % Show Material materials with Blei of 0.09 % |
Eisen | 0.25 % Show Material materials with Eisen of 0.25 % |
Kupfer | 85 - 90 % Show Material materials with Kupfer of 85 - 90 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Nickel | 4.5 - 6 % Show Material materials with Nickel of 4.5 - 6 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.05 % Show Material materials with Schwefel of 0.05 % |
Silizium | 5E-3 % Show Material materials with Silizium of 5E-3 % |
Zink | 1 - 2.5 % Show Material materials with Zink of 1 - 2.5 % |
Zinn | 4.5 - 6 % Show Material materials with Zinn of 4.5 - 6 % |