Mechanisch
Chemical properties
Property | Value |
---|---|
Aluminium | 0.1 % Show Material materials with Aluminium of 0.1 % |
Antimon | 0.02 % Show Material materials with Antimon of 0.02 % |
Bismut | 1E-3 % Show Material materials with Bismut of 1E-3 % |
Blei | 5E-3 % Show Material materials with Blei of 5E-3 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Mangan | 0.05 - 0.3 % Show Material materials with Mangan of 0.05 - 0.3 % |
Nickel | 9.5 - 10.5 % Show Material materials with Nickel of 9.5 - 10.5 % |
Phosphor | 5E-3 % Show Material materials with Phosphor of 5E-3 % |
Schwefel | 2.5E-3 % Show Material materials with Schwefel of 2.5E-3 % |
Silizium | 0.05 % Show Material materials with Silizium of 0.05 % |
Zink | 1 % Show Material materials with Zink of 1 % |
Zinn | 7.5 - 8.5 % Show Material materials with Zinn of 7.5 - 8.5 % |