Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 100 - 125 GPa Show Material materials with Elastizitätsmodul of 100 - 125 GPa | Typical for Wrought Copper Brass |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 50 - 67 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 50 - 67 [-] | |
Härte, Rockwell B | 23.0 °C | 51 - 70 [-] Show Material materials with Härte, Rockwell B of 51 - 70 [-] | |
Schubmodule | 23.0 °C | 40 GPa Show Material materials with Schubmodule of 40 GPa | Typical for Wrought Copper Brass |
Zugfestigkeit | 23.0 °C | 340 - 415 MPa Show Material materials with Zugfestigkeit of 340 - 415 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Wärmeleitfähigkeit | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |
Chemical properties
Property | Value |
---|---|
Blei | 0.09 % Show Material materials with Blei of 0.09 % |
Eisen | 0.05 % Show Material materials with Eisen of 0.05 % |
Kupfer | 89 - 92 % Show Material materials with Kupfer of 89 - 92 % |
Zinn | 0.3 - 0.7 % Show Material materials with Zinn of 0.3 - 0.7 % |