Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 52 - 63 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 52 - 63 [-] | |
Härte, Rockwell B | 23.0 °C | 49 - 69 [-] Show Material materials with Härte, Rockwell B of 49 - 69 [-] | |
Zugfestigkeit | 23.0 °C | 365 - 435 MPa Show Material materials with Zugfestigkeit of 365 - 435 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Schmelzpunkt | 855 - 1090 °C Show Material materials with Schmelzpunkt of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Blei | 0.03 % Show Material materials with Blei of 0.03 % |
Eisen | 2.1 - 2.6 % Show Material materials with Eisen of 2.1 - 2.6 % |
Kupfer | 97 % Show Material materials with Kupfer of 97 % |
Phosphor | 0.02 - 0.15 % Show Material materials with Phosphor of 0.02 - 0.15 % |
Zink | 0.05 - 0.2 % Show Material materials with Zink of 0.05 - 0.2 % |