Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.95 g/cm³ Show Material materials with Dichte of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 32 % Show Material materials with Dehnung A50 of 32 % | |
Elastizitätsmodul | 23.0 °C | 120 - 156 GPa Show Material materials with Elastizitätsmodul of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Yield strength Rp0.05 | 23.0 °C | 145 - 220 MPa Show Material materials with Yield strength Rp0.05 of 145 - 220 MPa | |
Zugfestigkeit | 23.0 °C | 380 - 480 MPa Show Material materials with Zugfestigkeit of 380 - 480 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Schmelzpunkt | 915 - 1240 °C Show Material materials with Schmelzpunkt of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade | |
Spezifische Wärmekapazität | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Wärmeleitfähigkeit | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Blei | 0.01 % Show Material materials with Blei of 0.01 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Nickel | 7 - 8 % Show Material materials with Nickel of 7 - 8 % |
Zink | 0.1 % Show Material materials with Zink of 0.1 % |
Zinn | 4.5 - 5.5 % Show Material materials with Zinn of 4.5 - 5.5 % |