Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.95 g/cm³ Show Material materials with Dichte of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 15 % Show Material materials with Dehnung A50 of 15 % | |
Elastizitätsmodul | 23.0 °C | 120 - 156 GPa Show Material materials with Elastizitätsmodul of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Streckgrenze Rp 0,2 | 23.0 °C | 90 - 110 MPa Show Material materials with Streckgrenze Rp 0,2 of 90 - 110 MPa | |
Yield strength Rp0.05 | 23.0 °C | 550 - 725 MPa Show Material materials with Yield strength Rp0.05 of 550 - 725 MPa | |
Zugfestigkeit | 23.0 °C | 725 - 860 MPa Show Material materials with Zugfestigkeit of 725 - 860 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Schmelzpunkt | 915 - 1240 °C Show Material materials with Schmelzpunkt of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade | |
Spezifische Wärmekapazität | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Wärmeleitfähigkeit | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Magnesium | 0.15 % Show Material materials with Magnesium of 0.15 % |
Mangan | 0.3 % Show Material materials with Mangan of 0.3 % |
Nickel | 14.5 - 15.5 % Show Material materials with Nickel of 14.5 - 15.5 % |
Niobium | 0.1 % Show Material materials with Niobium of 0.1 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 7.5 - 8.5 % Show Material materials with Zinn of 7.5 - 8.5 % |