Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 6 % Show Material materials with Dehnung A50 of 6 % |
Härte, Brinell | 20.0 °C | 190 [-] Show Material materials with Härte, Brinell of 190 [-] |
Streckgrenze Rp0,5 | 20.0 °C | 310 MPa Show Material materials with Streckgrenze Rp0,5 of 310 MPa |
Zugfestigkeit | 20.0 °C | 620 MPa Show Material materials with Zugfestigkeit of 620 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 10 - 11.5 % Show Material materials with Aluminium of 10 - 11.5 % |
Eisen | 3 - 5 % Show Material materials with Eisen of 3 - 5 % |
Kupfer | 83 % Show Material materials with Kupfer of 83 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 1.5 % Show Material materials with Nickel of 1.5 % |