Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 10 % Show Material materials with Dehnung A50 of 10 % | |
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 82 - 89 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 82 - 89 [-] | |
Härte, Rockwell B | 23.0 °C | 99 - 106 [-] Show Material materials with Härte, Rockwell B of 99 - 106 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 720 - 860 MPa Show Material materials with Streckgrenze Rp 0,2 of 720 - 860 MPa | |
Zugfestigkeit | 23.0 °C | 825 - 965 MPa Show Material materials with Zugfestigkeit of 825 - 965 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Schmelzpunkt | 855 - 1090 °C Show Material materials with Schmelzpunkt of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.2 % Show Material materials with Aluminium of 0.2 % |
Beryllium | 0.15 - 0.5 % Show Material materials with Beryllium of 0.15 - 0.5 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Nickel | 1 - 1.4 % Show Material materials with Nickel of 1 - 1.4 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Zinn | 0.25 % Show Material materials with Zinn of 0.25 % |
Zirkonium | 0.5 % Show Material materials with Zirkonium of 0.5 % |