Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.65 - 2.71 g/cm³ Show Material materials with Dichte of 2.65 - 2.71 g/cm³ | Typical for Cast 4xx.x Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastizitätsmodul | 71.0 - 75.0 GPa Show Material materials with Elastizitätsmodul of 71.0 - 75.0 GPa | Typical for Cast 4xx.x Series Aluminium | |||
Härte, Brinell | 40.0 [-] Show Material materials with Härte, Brinell of 40.0 [-] | F | ASTM B26 | Casting | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 4xx.x Series Aluminium | |||
Zugfestigkeit | 115.0 MPa Show Material materials with Zugfestigkeit of 115.0 MPa | F | ASTM B26 | Casting |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2e-05 - 2.2e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2e-05 - 2.2e-05 1/K | Typical for Cast 4xx.x Series Aluminium |
Schmelzpunkt | 565.0 - 630.0 °C Show Material materials with Schmelzpunkt of 565.0 - 630.0 °C | Typical for Cast 4xx.x Series Aluminium |
Spezifische Wärmekapazität | 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 963.0 J/(kg·K) | Typical for Cast 4xx.x Series Aluminium |
Wärmeleitfähigkeit | 130.0 - 170.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 - 170.0 W/(m·K) | Typical for Cast 4xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Eisen | 0.8 Show Material materials with Eisen of 0.8 | F | ASTM B26 | Casting |
Kupfer | 0.15 Show Material materials with Kupfer of 0.15 | F | ASTM B26 | Casting |
Magnesium | 0.05 Show Material materials with Magnesium of 0.05 | F | ASTM B26 | Casting |
Mangan | 0.35 Show Material materials with Mangan of 0.35 | F | ASTM B26 | Casting |
Silizium | 4.5 - 6.0 % Show Material materials with Silizium of 4.5 - 6.0 % | F | ASTM B26 | Casting |
Titan | 0.25 Show Material materials with Titan of 0.25 | F | ASTM B26 | Casting |
Zink | 0.35 Show Material materials with Zink of 0.35 | F | ASTM B26 | Casting |