Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7 g/cm³ Show Material materials with Dichte of 7 g/cm³ | Typical for Cast/Wrought Aluminium Zinc Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 8 - 9 % Show Material materials with Dehnung of 8 - 9 % | |
Dehnung A50 | 23.0 °C | 12 % Show Material materials with Dehnung A50 of 12 % | |
Elastizitätsmodul | 23.0 °C | 40 - 45 GPa Show Material materials with Elastizitätsmodul of 40 - 45 GPa | Typical for Cast/Wrought Aluminium Zinc Grade |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Zugfestigkeit | 23.0 °C | 221 - 275 MPa Show Material materials with Zugfestigkeit of 221 - 275 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.5E-5 - 2.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.5E-5 - 2.6E-5 1/K | Typical for Cast/Wrought Aluminium Zinc Grade |
Schmelzpunkt | 365 - 645 °C Show Material materials with Schmelzpunkt of 365 - 645 °C | Typical for Cast/Wrought Aluminium Zinc Grade | |
Spezifische Wärmekapazität | 23.0 °C | 800 - 1100 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 800 - 1100 J/(kg·K) | Typical for Cast/Wrought Aluminium Zinc Grade |
Wärmeleitfähigkeit | 23.0 °C | 44 - 110 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 44 - 110 W/(m·K) | Typical for Cast/Wrought Aluminium Zinc Grade |
Chemical properties
Property | Value |
---|---|
Aluminium | 2.5 - 3.5 % Show Material materials with Aluminium of 2.5 - 3.5 % |
Eisen | 5E-3 % Show Material materials with Eisen of 5E-3 % |
Kalzium | 0.04 % Show Material materials with Kalzium of 0.04 % |
Kupfer | 0.05 % Show Material materials with Kupfer of 0.05 % |
Mangan | 0.2 - 1 % Show Material materials with Mangan of 0.2 - 1 % |
Nickel | 5E-3 % Show Material materials with Nickel of 5E-3 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 0.6 - 1.4 % Show Material materials with Zink of 0.6 - 1.4 % |