Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 2.72 g/cm³ Show Material materials with Dichte of 2.72 g/cm³ | Typical for Cast Aluminium Manganese Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 6 % Show Material materials with Dehnung A50 of 6 % | |
Elastizitätsmodul | 23.0 °C | 40 - 45 GPa Show Material materials with Elastizitätsmodul of 40 - 45 GPa | Typical for Cast Aluminium Manganese Grade |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Streckgrenze | 23.0 °C | 140 MPa Show Material materials with Streckgrenze of 140 MPa | |
Zugfestigkeit | 23.0 °C | 210 MPa Show Material materials with Zugfestigkeit of 210 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.5E-5 - 2.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.5E-5 - 2.6E-5 1/K | Typical for Cast Aluminium Manganese Grade |
Schmelzpunkt | 465 - 620 °C Show Material materials with Schmelzpunkt of 465 - 620 °C | Typical for Cast Aluminium Manganese Grade | |
Spezifische Wärmekapazität | 23.0 °C | 1000 - 1080 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 1000 - 1080 J/(kg·K) | Typical for Cast Aluminium Manganese Grade |
Wärmeleitfähigkeit | 23.0 °C | 42 - 75 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 42 - 75 W/(m·K) | Typical for Cast Aluminium Manganese Grade |
Chemical properties
Property | Value |
---|---|
Aluminium | 3.5 - 5 % Show Material materials with Aluminium of 3.5 - 5 % |
Eisen | 3.5E-3 % Show Material materials with Eisen of 3.5E-3 % |
Kupfer | 0.02 % Show Material materials with Kupfer of 0.02 % |
Mangan | 0.35 - 0.7 % Show Material materials with Mangan of 0.35 - 0.7 % |
Nickel | 2E-3 % Show Material materials with Nickel of 2E-3 % |
Silizium | 0.5 - 1.5 % Show Material materials with Silizium of 0.5 - 1.5 % |
Zink | 0.12 % Show Material materials with Zink of 0.12 % |