Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7 g/cm³ Show Material materials with Dichte of 7 g/cm³ | Typical for Cast/Wrought Aluminium Zinc Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 7 - 9 % Show Material materials with Dehnung A50 of 7 - 9 % | |
Elastizitätsmodul | 23.0 °C | 44.8 GPa Show Material materials with Elastizitätsmodul of 44.8 GPa | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Streckgrenze Rp 0,2 | 23.0 °C | 110 - 165 MPa Show Material materials with Streckgrenze Rp 0,2 of 110 - 165 MPa | |
Zugfestigkeit | 23.0 °C | 250 - 275 MPa Show Material materials with Zugfestigkeit of 250 - 275 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.5E-5 - 2.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.5E-5 - 2.6E-5 1/K | Typical for Cast/Wrought Aluminium Zinc Grade |
Schmelzpunkt | 365 - 645 °C Show Material materials with Schmelzpunkt of 365 - 645 °C | Typical for Cast/Wrought Aluminium Zinc Grade | |
Spezifische Wärmekapazität | 23.0 °C | 800 - 1100 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 800 - 1100 J/(kg·K) | Typical for Cast/Wrought Aluminium Zinc Grade |
Wärmeleitfähigkeit | 23.0 °C | 44 - 110 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 44 - 110 W/(m·K) | Typical for Cast/Wrought Aluminium Zinc Grade |
Chemical properties
Property | Value |
---|---|
Aluminium | 5.8 - 7.2 % Show Material materials with Aluminium of 5.8 - 7.2 % |
Eisen | 5E-3 % Show Material materials with Eisen of 5E-3 % |
Kupfer | 0.05 % Show Material materials with Kupfer of 0.05 % |
Mangan | 0.15 - 0.5 % Show Material materials with Mangan of 0.15 - 0.5 % |
Nickel | 5E-3 % Show Material materials with Nickel of 5E-3 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 0.4 - 1.5 % Show Material materials with Zink of 0.4 - 1.5 % |