Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.18 g/cm³ Show Material materials with Dichte of 7.18 g/cm³ | Typical for Wrought Zinc Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 4 % Show Material materials with Dehnung A50 of 4 % | |
Elastizitätsmodul | 23.0 °C | 44.8 GPa Show Material materials with Elastizitätsmodul of 44.8 GPa | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Streckgrenze Rp 0,2 | 23.0 °C | 235 - 255 MPa Show Material materials with Streckgrenze Rp 0,2 of 235 - 255 MPa | |
Zugfestigkeit | 23.0 °C | 255 - 275 MPa Show Material materials with Zugfestigkeit of 255 - 275 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.7E-5 - 2.72E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.7E-5 - 2.72E-5 1/K | Typical for Wrought Zinc Grade |
Schmelzpunkt | 520 - 635 °C Show Material materials with Schmelzpunkt of 520 - 635 °C | Typical for Wrought Zinc Grade | |
Spezifische Wärmekapazität | 23.0 °C | 1050 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 1050 J/(kg·K) | Typical for Wrought Zinc Grade |
Wärmeleitfähigkeit | 23.0 °C | 117 - 146 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 117 - 146 W/(m·K) | Typical for Wrought Zinc Grade |
Chemical properties
Property | Value |
---|---|
Zink | 3.5 - 4.5 % Show Material materials with Zink of 3.5 - 4.5 % |
Zirkonium | 0.45 % Show Material materials with Zirkonium of 0.45 % |