Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.8 g/cm³ Show Material materials with Dichte of 2.8 g/cm³ | Typical for Cast 7xx.x Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 6.0 % Show Material materials with Dehnung of 6.0 % | T1 | ASTM B108 | Casting | |
Elastizitätsmodul | 74.0 GPa Show Material materials with Elastizitätsmodul of 74.0 GPa | Typical for Cast 7xx.x Series Aluminium | |||
Härte, Brinell | 70.0 [-] Show Material materials with Härte, Brinell of 70.0 [-] | T1 | ASTM B108 | Casting | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 7xx.x Series Aluminium | |||
Zugfestigkeit | 195.0 MPa Show Material materials with Zugfestigkeit of 195.0 MPa | T1 | ASTM B108 | Casting |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.4e-05 - 2.5e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.4e-05 - 2.5e-05 1/K | Typical for Cast 7xx.x Series Aluminium |
Schmelzpunkt | 550.0 - 645.0 °C Show Material materials with Schmelzpunkt of 550.0 - 645.0 °C | Typical for Cast 7xx.x Series Aluminium |
Spezifische Wärmekapazität | 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 963.0 J/(kg·K) | Typical for Cast 7xx.x Series Aluminium |
Wärmeleitfähigkeit | 100.0 - 160.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 100.0 - 160.0 W/(m·K) | Typical for Cast 7xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Eisen | 0.7 - 1.4 % Show Material materials with Eisen of 0.7 - 1.4 % | T1 | ASTM B108 | Casting |
Kupfer | 0.35 - 0.6 % Show Material materials with Kupfer of 0.35 - 0.6 % | T1 | ASTM B108 | Casting |
Magnesium | 0.25 - 0.45 % Show Material materials with Magnesium of 0.25 - 0.45 % | T1 | ASTM B108 | Casting |
Mangan | 0.05 Show Material materials with Mangan of 0.05 | T1 | ASTM B108 | Casting |
Silizium | 0.3 Show Material materials with Silizium of 0.3 | T1 | ASTM B108 | Casting |
Titan | 0.2 Show Material materials with Titan of 0.2 | T1 | ASTM B108 | Casting |
Zink | 6.0 - 7.0 % Show Material materials with Zink of 6.0 - 7.0 % | T1 | ASTM B108 | Casting |