Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.7 g/cm³ Show Material materials with Dichte of 1.7 g/cm³ | Typical for Cast Rare Earth Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 2 % Show Material materials with Dehnung A50 of 2 % | |
Elastizitätsmodul | 23.0 °C | 40 - 45 GPa Show Material materials with Elastizitätsmodul of 40 - 45 GPa | Typical for Cast Rare Earth Grade |
Härte, Brinell | 23.0 °C | 50 [-] Show Material materials with Härte, Brinell of 50 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Streckgrenze Rp 0,2 | 23.0 °C | 96 MPa Show Material materials with Streckgrenze Rp 0,2 of 96 MPa | |
Zugfestigkeit | 23.0 °C | 138 MPa Show Material materials with Zugfestigkeit of 138 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.6E-5 1/K | Typical for Cast Rare Earth Grade |
Schmelzpunkt | 535 - 645 °C Show Material materials with Schmelzpunkt of 535 - 645 °C | Typical for Cast Rare Earth Grade | |
Spezifische Wärmekapazität | 23.0 °C | 966 - 1050 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 966 - 1050 J/(kg·K) | Typical for Cast Rare Earth Grade |
Wärmeleitfähigkeit | 23.0 °C | 51 - 113 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 51 - 113 W/(m·K) | Typical for Cast Rare Earth Grade |
Chemical properties
Property | Value |
---|---|
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % |
Nickel | 0.01 % Show Material materials with Nickel of 0.01 % |
Seltene-Erden-Elemente | 2.5 - 4 % Show Material materials with Seltene-Erden-Elemente of 2.5 - 4 % |
Zink | 2 - 3.1 % Show Material materials with Zink of 2 - 3.1 % |
Zirkonium | 0.5 - 1 % Show Material materials with Zirkonium of 0.5 - 1 % |