Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | Typical for Wrought 1000 Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 22.0 % Show Material materials with Dehnung of 22.0 % | O | ASTM B241 | Tube | |
25.0 % Show Material materials with Dehnung of 25.0 % | O | ASTM B241 | Tube | A50 | |
Elastizitätsmodul | 68.0 - 70.0 GPa Show Material materials with Elastizitätsmodul of 68.0 - 70.0 GPa | Typical for Wrought 1000 Series Aluminium | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | |||
Schubmodule | 25.9 GPa Show Material materials with Schubmodule of 25.9 GPa | Typical for Wrought 1000 Series Aluminium | |||
Zugfestigkeit | 75.0 - 105.0 MPa Show Material materials with Zugfestigkeit of 75.0 - 105.0 MPa | O | ASTM B241 | Tube |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.2e-05 - 2.5e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 1000 Series Aluminium |
Schmelzpunkt | 645.0 - 660.0 °C Show Material materials with Schmelzpunkt of 645.0 - 660.0 °C | Typical for Wrought 1000 Series Aluminium |
Spezifische Wärmekapazität | 900.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 900.0 - 963.0 J/(kg·K) | Typical for Wrought 1000 Series Aluminium |
Wärmeleitfähigkeit | 167.0 - 244.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 167.0 - 244.0 W/(m·K) | Typical for Wrought 1000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 33000000.0 - 38000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 33000000.0 - 38000000.0 S/m | Typical for Wrought 1000 Series Aluminium |
spezifischer Widerstand | 2.7e-08 - 3e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.7e-08 - 3e-08 Ω·m | Typical for Wrought 1000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 99.0 % Show Material materials with Aluminium of 99.0 % | O | ASTM B241 | Tube |
Kupfer | 0.05 - 0.2 % Show Material materials with Kupfer of 0.05 - 0.2 % | O | ASTM B241 | Tube |
Mangan | 0.05 Show Material materials with Mangan of 0.05 | O | ASTM B241 | Tube |
Silizium | 0.95 Show Material materials with Silizium of 0.95 | O | ASTM B241 | Tube |
Zink | 0.1 Show Material materials with Zink of 0.1 | O | ASTM B241 | Tube |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |