Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.74 g/cm³ Show Material materials with Dichte of 1.74 g/cm³ | Typical for Magnesium |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 2.5 % Show Material materials with Dehnung of 2.5 % | |
Elastizitätsmodul | 23.0 °C | 45 GPa Show Material materials with Elastizitätsmodul of 45 GPa | Typical for Magnesium |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Streckgrenze Rp 0,2 | 23.0 °C | 133 MPa Show Material materials with Streckgrenze Rp 0,2 of 133 MPa | |
Zugfestigkeit | 23.0 °C | 200 MPa Show Material materials with Zugfestigkeit of 200 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.3E-5 - 2.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 - 2.6E-5 1/K | Typical for Magnesium |
Schmelzpunkt | 650 °C Show Material materials with Schmelzpunkt of 650 °C | Typical for Magnesium | |
Spezifische Wärmekapazität | 23.0 °C | 1010 - 1060 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 1010 - 1060 J/(kg·K) | Typical for Magnesium |
Wärmeleitfähigkeit | 23.0 °C | 153 - 167 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 153 - 167 W/(m·K) | Typical for Magnesium |
Chemical properties
Property | Value |
---|---|
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % |
Mangan | 0.15 % Show Material materials with Mangan of 0.15 % |
Nickel | 0.01 % Show Material materials with Nickel of 0.01 % |
Seltene-Erden-Elemente | 0.75 - 1.75 % Show Material materials with Seltene-Erden-Elemente of 0.75 - 1.75 % |
Zink | 3.5 - 5 % Show Material materials with Zink of 3.5 - 5 % |
Zirkonium | 0.4 - 1 % Show Material materials with Zirkonium of 0.4 - 1 % |