Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 2.65 - 2.7 g/cm³ Show Material materials with Dichte of 2.65 - 2.7 g/cm³ | Typical for Wrought 5000 Series Aluminium |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Bruchfestigkeit | 20.0 °C | 22 - 35 MPa·√m Show Material materials with Bruchfestigkeit of 22 - 35 MPa·√m | Typical for Wrought 5000 Series Aluminium |
Elastizitätsmodul | 20.0 °C | 69 - 70 GPa Show Material materials with Elastizitätsmodul of 69 - 70 GPa | Typical for Wrought 5000 Series Aluminium |
Poissonzahl | 20.0 °C | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 5000 Series Aluminium |
Schubmodule | 20.0 °C | 26 - 26.5 GPa Show Material materials with Schubmodule of 26 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 2.2E-5 - 2.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2E-5 - 2.5E-5 1/K | Typical for Wrought 5000 Series Aluminium |
Max. Betriebstemperatur | 150 °C Show Material materials with Max. Betriebstemperatur of 150 °C | Typical for Wrought 5000 Series Aluminium | |
Schmelzpunkt | 600 - 650 °C Show Material materials with Schmelzpunkt of 600 - 650 °C | Typical for Wrought 5000 Series Aluminium | |
Spezifische Wärmekapazität | 20.0 °C | 879 - 963 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 879 - 963 J/(kg·K) | Typical for Wrought 5000 Series Aluminium |
Wärmeleitfähigkeit | 20.0 °C | 112 - 205 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 112 - 205 W/(m·K) | Typical for Wrought 5000 Series Aluminium |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1.80E+7 - 3.10E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.80E+7 - 3.10E+7 S/m | Typical for Wrought 5000 Series Aluminium |
spezifischer Widerstand | 20.0 °C | 3.3E-8 - 5E-8 Ω·m Show Material materials with spezifischer Widerstand of 3.3E-8 - 5E-8 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value |
---|---|
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Magnesium | 0.5 - 1.1 % Show Material materials with Magnesium of 0.5 - 1.1 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % |
Zink | 0.25 % Show Material materials with Zink of 0.25 % |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |