Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | Typical for Wrought 6000 Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 16.0 % Show Material materials with Dehnung of 16.0 % | T4, T42 | ASTM B483 | Tube | A50 |
16.0 % Show Material materials with Dehnung of 16.0 % | T4, T42 | ASTM B483 | Tube | ||
18.0 % Show Material materials with Dehnung of 18.0 % | T4, T42 | ASTM B483 | Tube | A50 | |
20.0 % Show Material materials with Dehnung of 20.0 % | T4, T42 | ASTM B483 | Tube | A50 | |
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | Typical for Wrought 6000 Series Aluminium | |||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | |||
Schubmodule | 26.0 - 26.5 GPa Show Material materials with Schubmodule of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | |||
Zugfestigkeit | 150.0 MPa Show Material materials with Zugfestigkeit of 150.0 MPa | T4, T42 | ASTM B483 | Tube |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 6000 Series Aluminium |
Schmelzpunkt | 555.0 - 655.0 °C Show Material materials with Schmelzpunkt of 555.0 - 655.0 °C | Typical for Wrought 6000 Series Aluminium |
Spezifische Wärmekapazität | 887.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 887.0 - 963.0 J/(kg·K) | Typical for Wrought 6000 Series Aluminium |
Wärmeleitfähigkeit | 170.0 - 220.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 170.0 - 220.0 W/(m·K) | Typical for Wrought 6000 Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 21000000.0 - 34000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 21000000.0 - 34000000.0 S/m | Typical for Wrought 6000 Series Aluminium |
spezifischer Widerstand | 2.9e-08 - 5e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.9e-08 - 5e-08 Ω·m | Typical for Wrought 6000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.1 Show Material materials with Chrom of 0.1 | T4, T42 | ASTM B483 | Tube |
Eisen | 0.35 Show Material materials with Eisen of 0.35 | T4, T42 | ASTM B483 | Tube |
Kupfer | 0.1 Show Material materials with Kupfer of 0.1 | T4, T42 | ASTM B483 | Tube |
Magnesium | 0.45 - 0.9 % Show Material materials with Magnesium of 0.45 - 0.9 % | T4, T42 | ASTM B483 | Tube |
Mangan | 0.1 Show Material materials with Mangan of 0.1 | T4, T42 | ASTM B483 | Tube |
Silizium | 0.2 - 0.6 % Show Material materials with Silizium of 0.2 - 0.6 % | T4, T42 | ASTM B483 | Tube |
Titan | 0.1 Show Material materials with Titan of 0.1 | T4, T42 | ASTM B483 | Tube |
Zink | 0.1 Show Material materials with Zink of 0.1 | T4, T42 | ASTM B483 | Tube |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |