Property | Value | Comment |
---|---|---|
Dichte | 2.8 g/cm³ Show Material materials with Dichte of 2.8 g/cm³ | Typical for Cast 8xx.x Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 3.0 % Show Material materials with Dehnung of 3.0 % | T5 | ASTM B618 | Casting | |
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | Typical for Cast 8xx.x Series Aluminium | |||
Härte, Brinell | 45.0 [-] Show Material materials with Härte, Brinell of 45.0 [-] | T5 | ASTM B618 | Casting | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 8xx.x Series Aluminium | |||
Zugfestigkeit | 115.0 MPa Show Material materials with Zugfestigkeit of 115.0 MPa | T5 | ASTM B618 | Casting |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | Typical for Cast 8xx.x Series Aluminium |
Schmelzpunkt | 205.0 - 650.0 °C Show Material materials with Schmelzpunkt of 205.0 - 650.0 °C | Typical for Cast 8xx.x Series Aluminium |
Spezifische Wärmekapazität | 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 963.0 J/(kg·K) | Typical for Cast 8xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Eisen | 0.7 Show Material materials with Eisen of 0.7 | T5 | ASTM B618 | Casting |
Kupfer | 0.7 - 1.3 % Show Material materials with Kupfer of 0.7 - 1.3 % | T5 | ASTM B618 | Casting |
Magnesium | 0.1 Show Material materials with Magnesium of 0.1 | T5 | ASTM B618 | Casting |
Mangan | 0.1 Show Material materials with Mangan of 0.1 | T5 | ASTM B618 | Casting |
Nickel | 0.3 - 0.7 % Show Material materials with Nickel of 0.3 - 0.7 % | T5 | ASTM B618 | Casting |
Silizium | 2.0 - 3.0 % Show Material materials with Silizium of 2.0 - 3.0 % | T5 | ASTM B618 | Casting |
Titan | 0.2 Show Material materials with Titan of 0.2 | T5 | ASTM B618 | Casting |
Zinn | 5.5 - 7.0 % Show Material materials with Zinn of 5.5 - 7.0 % | T5 | ASTM B618 | Casting |