Property | Value | Comment |
---|---|---|
Dichte | 2.75 - 2.8 g/cm³ Show Material materials with Dichte of 2.75 - 2.8 g/cm³ | Typical for Cast 2xx.x Series Aluminium |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 3.0 % Show Material materials with Dehnung of 3.0 % | Class 1, Specimens Cut from Designated Areas of Casting | ASTM B686 | Casting | |
Elastizitätsmodul | 72.0 GPa Show Material materials with Elastizitätsmodul of 72.0 GPa | Typical for Cast 2xx.x Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 2xx.x Series Aluminium | |||
Streckgrenze | 345.0 MPa Show Material materials with Streckgrenze of 345.0 MPa | Class 1, Specimens Cut from Designated Areas of Casting | ASTM B686 | Casting | |
Zugfestigkeit | 415.0 MPa Show Material materials with Zugfestigkeit of 415.0 MPa | Class 1, Specimens Cut from Designated Areas of Casting | ASTM B686 | Casting |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.9e-05 - 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.9e-05 - 2.3e-05 1/K | Typical for Cast 2xx.x Series Aluminium |
Schmelzpunkt | 510.0 - 790.0 °C Show Material materials with Schmelzpunkt of 510.0 - 790.0 °C | Typical for Cast 2xx.x Series Aluminium |
Spezifische Wärmekapazität | 875.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 875.0 - 963.0 J/(kg·K) | Typical for Cast 2xx.x Series Aluminium |
Wärmeleitfähigkeit | 120.0 - 150.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 120.0 - 150.0 W/(m·K) | Typical for Cast 2xx.x Series Aluminium |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 16000000.0 - 23000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 16000000.0 - 23000000.0 S/m | Typical for Cast 2xx.x Series Aluminium |
spezifischer Widerstand | 4.347826086956522e-08 - 6.25e-08 Ω·m Show Material materials with spezifischer Widerstand of 4.347826086956522e-08 - 6.25e-08 Ω·m | Typical for Cast 2xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Eisen | 0.1 Show Material materials with Eisen of 0.1 | Class 1, Specimens Cut from Designated Areas of Casting | ASTM B686 | Casting |
Kupfer | 4.0 - 5.0 % Show Material materials with Kupfer of 4.0 - 5.0 % | Class 1, Specimens Cut from Designated Areas of Casting | ASTM B686 | Casting |
Magnesium | 0.15 - 0.35 % Show Material materials with Magnesium of 0.15 - 0.35 % | Class 1, Specimens Cut from Designated Areas of Casting | ASTM B686 | Casting |
Mangan | 0.2 - 0.4 % Show Material materials with Mangan of 0.2 - 0.4 % | Class 1, Specimens Cut from Designated Areas of Casting | ASTM B686 | Casting |
Silber | 0.4 - 1.0 % Show Material materials with Silber of 0.4 - 1.0 % | Class 1, Specimens Cut from Designated Areas of Casting | ASTM B686 | Casting |
Silizium | 0.05 Show Material materials with Silizium of 0.05 | Class 1, Specimens Cut from Designated Areas of Casting | ASTM B686 | Casting |
Titan | 0.15 - 0.35 % Show Material materials with Titan of 0.15 - 0.35 % | Class 1, Specimens Cut from Designated Areas of Casting | ASTM B686 | Casting |