Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Duplex Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 18 % Show Material materials with Dehnung of 18 % | |
Elastizitätsmodul | 23.0 °C | 200 GPa Show Material materials with Elastizitätsmodul of 200 GPa | Typical for Duplex Stainless Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Duplex Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Duplex Stainless Steel |
Streckgrenze | 23.0 °C | 392 MPa Show Material materials with Streckgrenze of 392 MPa | |
Zugfestigkeit | 23.0 °C | 588 MPa Show Material materials with Zugfestigkeit of 588 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 1/K | Typical for Duplex Stainless Steel |
Max. Betriebstemperatur | 300 °C Show Material materials with Max. Betriebstemperatur of 300 °C | Typical for Duplex Stainless Steel | |
Schmelzpunkt | 1375 - 1450 °C Show Material materials with Schmelzpunkt of 1375 - 1450 °C | Typical for Duplex Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 440 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 - 502 J/(kg·K) | Typical for Duplex Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 13 - 30 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 13 - 30 W/(m·K) | Typical for Duplex Stainless Steel |
Technological properties
Property | ||
---|---|---|
Processing history | hot-rolled and solution annealed |