Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 6.8 - 7.8 g/cm³ Show Material materials with Dichte of 6.8 - 7.8 g/cm³ | Typical for Cast Iron |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 12 % Show Material materials with Dehnung of 12 % | |
Elastizitätsmodul | 23.0 °C | 152 GPa Show Material materials with Elastizitätsmodul of 152 GPa | |
Härte, HBW | 23.0 °C | 156 - 217 [-] Show Material materials with Härte, HBW of 156 - 217 [-] | |
Poissonzahl | 23.0 °C | 0.27 [-] Show Material materials with Poissonzahl of 0.27 [-] | Typical for Cast Iron |
Schubmodule | 23.0 °C | 41 GPa Show Material materials with Schubmodule of 41 GPa | Typical for Cast Iron |
Streckgrenze | 23.0 °C | 285 - 310 MPa Show Material materials with Streckgrenze of 285 - 310 MPa | |
Zugfestigkeit | 23.0 °C | 450 MPa Show Material materials with Zugfestigkeit of 450 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 1120 °C Show Material materials with Schmelzpunkt of 1120 °C | Typical for Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 - 527 J/(kg·K) | Typical for Cast Iron |
Wärmeleitfähigkeit | 23.0 °C | 55 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 55 W/(m·K) | Typical for Cast Iron |
Chemical properties
Property | Value |
---|---|
Eisen | balance |
Kohlenstoff | 3.2 - 4.1 % Show Material materials with Kohlenstoff of 3.2 - 4.1 % |
Mangan | 0.1 - 1 % Show Material materials with Mangan of 0.1 - 1 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.005 - 0.035 % Show Material materials with Schwefel of 0.005 - 0.035 % |
Silizium | 1.8 - 3 % Show Material materials with Silizium of 1.8 - 3 % |