Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 6.8 - 7.8 g/cm³ Show Material materials with Dichte of 6.8 - 7.8 g/cm³ | Typical for Cast Iron |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 152 GPa Show Material materials with Elastizitätsmodul of 152 GPa | Typical for Cast Iron |
Poissonzahl | 23.0 °C | 0.27 [-] Show Material materials with Poissonzahl of 0.27 [-] | Typical for Cast Iron |
Schubmodule | 23.0 °C | 41 GPa Show Material materials with Schubmodule of 41 GPa | Typical for Cast Iron |
Zugfestigkeit | 20.0 °C | 100 MPa Show Material materials with Zugfestigkeit of 100 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 1120 °C Show Material materials with Schmelzpunkt of 1120 °C | Typical for Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 - 527 J/(kg·K) | Typical for Cast Iron |
Wärmeleitfähigkeit | 23.0 °C | 55 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 55 W/(m·K) | Typical for Cast Iron |